FPM FKM Pre-compounding BDF30P
BDF30P
BODA Fluoroelastomer BDF30P | ||||||
Technical Data Sheet | CHENGDU CHENGUANG FLUORO-SLIICONE ELASTOMER CO., LTD | |||||
BDF30P is a low to medium viscosity curative incorporated fluoroelastomer copolymer. This is a general purpose grade, well suited for application where good flowability and mold release are required. BDF30P can be compounded to meet the major fluoroelastomer specifications. BDF30P can be used for compression molding of O-ring and gasket or extrusion of complex geometries. It can be mixed using typical fluoroelastomer compounding ingredients. Mixing can be accomplished with two-roll mills or internal mixers. Finished goods can be produced by a variety of rubber processing methods. Basic characteristics of the polymer are as follows: | ||||||
Properties | Typical Values | |||||
Fluorine Content, % | 66 | |||||
Specific Gravity | 1.80 | |||||
Color | White | |||||
Solubility | LMW Ketones and esters | |||||
Mooney Viscosity ML | 30 | |||||
Typical Properties of BDF30P | ||||||
Test Compound | ||||||
Polymer | 100 | |||||
MT Black (N990) | phr | 30 | ||||
MgO | Phr | 3 | ||||
Ca(OH)2 | phr | 6 | ||||
Curing Condition | Press | 10min at 170C | ||||
Oven | 24h at 230C | |||||
Typical Rheological Properties Monsanto Moving Die Rheometer (MDR2000®) 100cpm, 0.5°Arc, 6 minutes, 177C |
| |||||
ML, Minimum Torque | N m | 0.30 | ||||
ts2, Time to 2 inch-lb rise from minimum | 1' 00'' | |||||
t90, Time to 90% cure | 2' 10'' | |||||
MH, Maximum Torque | N m | 1.85 | ||||
Typcial Physical Properties Press Cure 10 minutes @ 170 Post Cure 24 hours @ 230 |
|
| ||||
Tensile (ASTM D412) | Mpa | 13.5 | ||||
Elongation at break (ASTM D412) | % | 230 | ||||
Hardness (ASTM D2240) | Shore A | 78 | ||||
Compression Set, [ASTM D395 Method B (Disc)] | ||||||
Aged 70 hours @ 200C | % | 18 | ||||
Because conditions of product use are outside s control and vary widely, User must evaluate and determine whether a Boda product will be suitable for users intended application before using it. The following is made in lieu in all express and implied warranties (including warranties of merchantability and fitness for a particular purpose): If a Boda product is proved to be defective, Bodas only obligation, and users only remedy, will be, at Bodas option, to replace the quantity of product shown to be defective when user received it or to refund users purchase price. In no event will Boda be liable for any direct, indirect, special, incidental, or consequential loss or damage, regardless of legal theory, such as breach of warranty or contract, negligence, or strict liability. |